Show simple item record

dc.contributorNevstad, Gunnar Oveen_GB
dc.date.accessioned2018-10-29T13:29:13Z
dc.date.available2018-10-29T13:29:13Z
dc.date.issued2005
dc.identifier
dc.identifier.isbn82-464-0965-4en_GB
dc.identifier.other2005/00005
dc.identifier.urihttp://hdl.handle.net/20.500.12242/1788
dc.description.abstractPBXN-110 a cast cure PBX containing an inert binder system and HMX has been studied with regard to process ability by use of different ratios between HMX class 2 and class 3. A ratio of 30:70 between HMX class 2 and class 3 was found to give the lowest viscosity and cured samples with satisfactory hardness. With a ratio of 30:70 between class 2 and class 3 and a filler content of 87.2 weight% Intermediate Scale Gap test tubes was filled. The cured material had satisfactory density of 1.64 g/cm3. 10 tubes with different barrier thickness were fired to determine the shock sensitivity. For the 50% probability of a detonation we obtained a limit between go/no go of 35.5+1 kbar. A shock sensitivity result for PBXN-110 in agreement with literature values.en_GB
dc.language.isonoben_GB
dc.titleEgenskaper til PBXN-110 med standard HMXen_GB
dc.subject.keywordSprengstoffer - Følsomheten_GB
dc.source.issue2005/00005en_GB
dc.source.pagenumber43en_GB