dc.description.abstract | Octol 60/40 and 70/30 (HMX/TNT) have been tested with regard to shock sensitivity in
Intermediate Scale GAP test. Both compositions were cast filled into the test tubes. An average
density of 98.1% of TMD was obtained for the fillings with Octol 60/40 and 98.2 % of TMD for
the fillings with Octol 70/30.
The shock sensitivity for Octol 60/40 was found to be 14.5 kbar and for Octol 70/30 16.0 kbar,
indicating that Octol 60/40 is slightly more shock sensitive than Octol 70/30. | en_GB |
dc.description.abstract | Oktol 60/40 og Oktol 70/30 (HMX/TNT) har blitt testet med hensyn på sjokkfølsomhet i
Intermediate Scale GAP test. Begge komposisjonene ble smeltestøpt i test rørene. En
gjennomsnittlig tetthet på 98.1% av TMD ble oppnådd for fyllingene med Oktol 60/40 og 98.2%
av TMD for fyllingene med Oktol 70/30.
Sjokkfølsomheten ble funnet å være 14.5 kbar for Oktol 60/40 og 16.0 kbar for Oktol 70/30. Et
resultat som gir Oktol 60/40 en noe høyere sjokkfølsomhet enn Oktol 70/30. | en_GB |
dc.language.iso | en | en_GB |
dc.title | Shock sensitivity testing of Octols | en_GB |
dc.subject.keyword | Sprengstoffer - Følsomhet | en_GB |
dc.source.issue | 2008/00468 | en_GB |
dc.source.pagenumber | 75 | en_GB |